Duplex TIG
TIG welding of duplex and super duplex stainless steel for desalination plants, ships and refineries, across all wall thicknesses, with controlled heat input.
Material
Duplex and super duplex stainless steels for corrosive seawater service.
- Duplex stainless steel
- Super duplex stainless steel
- All wall thicknesses
- Seawater and process service



Welding
Every joint was welded with TIG and super duplex filler metal.
- TIG (GTAW) welding
- Filler 25 9 4 N L
- Qualified procedures
- Multi-pass welding



Heat Input
Heat input and interpass temperature were kept within tight limits.
- Controlled heat input
- Interpass temperature control
- Balanced weld structure
- Corrosion resistance kept



Purging
Back purging with argon protected the root on every pipe joint.
- Argon back purging
- Clean, oxide-free root
- Low oxygen at the root
- Desalination, ships, refineries



Qualified
Welder qualified to EN ISO 9606-1 for duplex with super duplex filler.
- EN ISO 9606-1, group 10.1
- Super duplex filler metal
- Duplex certified since 2017
- Work to project requirements